RESISTANCE OF COMPACTED ASPHALT
MIXTURES TO MOISTURE-INDUCED DAMAGE
AASHTO T 283
GLOSSARY
Tensile strength -- a measure of the force required to pull apart a material.
SCOPE
HMA made from certain materials may be sensitive to the presence of water in the finished
pavement. Water will cause the binder to not adhere to the aggregate. Since the binder is the
glue that holds the pavement together, rapid failure of the pavement can be expected if the
binder cannot adhere to the aggregate. This is often referred to as stripping. To help prevent
stripping, additives such as hydrated lime or liquid anti-stripping chemicals may be required.
AASHTO T 283 is a test method that can be used to determine if the materials may be subject to
stripping and also to measure the effectiveness of additives.
The test is performed by compacting specimens to an air void level of six to eight percent. Three
specimens are selected as a control and tested without moisture conditioning, and three more
specim,ens are selected to be conditioned by saturating with water undergoing a freeze cycle, and
subsequently having a warm-water soaking cycle. The specimens are then tested for indirect
tensile strength by loading the specimens at a constant rate and measuring the force required to
break the specimen. The tensile strength of the conditioned specimens is compared to the control
specimens to determine the tensile strength ratio (TSR). This test may also be performed on
cores taken from the finished pavement.
SUMMARY OF TEST
Apparatus
Vacuum container for saturating specimens
Balance, general purpose class G2 (AASHTO M 231)
Water bath, capable of maintaining a temperature of 140 ± 2°F (60 ± 1°C)
您可能关注的文档
- API MPMS 12.2.5-2001(R2011) 石 油计量标准手册 第12章石 油量计算第2.5节-使用动态测量方法和体 积校正系数计算石 油量.pdf
- API MPMS 12.2.4-1997(R2009) 石 油计量标准手册 第12章石油量的计算第2.4节-使用动态测量方法和体积修正系数计算石油量.pdf
- AASHTO R28-02 压力老化试验规范.pdf
- AASHTO T89 土的液限值测试方法.pdf
- AASHTO T160-93 水泥砂浆和混凝土硬化后长度的改变.pdf
- AASHTO T167-94 混合料试件的压缩强度.pdf
- AASHTO T209 沥青混合料理论最大密度试验方法.pdf
- GM 269M-2012 发动机舱声降噪结构.pdf
- GM 2617M-2003 内饰零件性能.pdf
- GM 2617M-2005 内饰零件性能.pdf
文档评论(0)